Skip to main content
. 2012 Oct 30;14(11):1246. doi: 10.1007/s11051-012-1246-1

Fig. 18.

Fig. 18

Decane droplet on quartz plate immersed in a water and b 5 nm quat/PEG (50:50)-modified silica nanoparticle dispersion of 1 wt%. The contact angle is a 91° and b 14°