Skip to main content
. 2012 Oct 30;14(11):1246. doi: 10.1007/s11051-012-1246-1

Fig. 22.

Fig. 22

Decane droplet on quartz plate immersed in a water and b 25 nm PEG-modified silica nanoparticle dispersion of 1 wt%. The contact angle is a 56° and b 51°