Fig. 7.

Fig. 7

Ligand density on antigen-labeled Au nanoparticles with co-adsorbed PEG, characterized by an antibody-functionalized AFM probe tip (inset, upper left). As the PEG size increases, the number of measureable ligand–receptor interactions decreases (F ~180 pN), with a commensurate rise in nonspecific substrate–tip interactions (F ~20 pN).