Table 1.

Summary of Material Characterizationa

sample swelling ratio mesh size (Å) storage modulus (Pa) loss modulus (Pa)
10% PEGDM 13.5 ± 1.0 120.2 ± 7.0 1578 ± 60 793 ± 78
10% PEGDM + 1% Col I 13.2 ± 1.1b 114.4 ± 6.2 2214 ± 189 545 ± 103b
10% PEGDM + 1% Col I + 0.5% HA 15.9 ± 0.4c 132.7 ± 1.8b 1275 ± 51c 852 ± 109
10% PEGDM + 1% Col I + 1.0% HA 13.3 ± 1.9 112.3 ± 6.5 1238 ± 34c 865 ± 6
a

All data points are reported as average ± standard deviation.

b

Indicates a p-value <0.05 relative to 10% PEGDM samples.

c

Indicates p-value <0.01 relative to 10% PEGDM samples.