. 2012 Dec 7;2:939. doi: 10.1038/srep00939

Table 2. Comparison between the calculated and experimental Poisson's ratio for the cases of 29.6-nm- and 155.8-nm-thick (Ba,Sr)TiO3 films grown at 505°C.

  ε00 εz0 −εz0
  Calc. (10−12 m2/N) Calc. Meas. (at 29.6 nm) Meas. (155.8 nm)
[002] 4.047 −3.439 0.850 0.942 0.942
[110] 3.240 −1.824 0.563 0.454 0.454
[111] 2.971 −1.286 0.433 0.342 0.342