Figure 1.

Figure 1

The surface density of grafted PSAR-20 chains (left axis) and the corresponding brush thickness in the dry-state as measured by ellipsometry (right axis). A wide range of surface chain densities was achieved by solution grafting of PSAR-20 from varying solution concentrations and durations of exposure. The error bars indicate ±1 SD.