Skip to main content
. 2012 Dec 24;2012:198351. doi: 10.5402/2012/198351

Table 2.

Temperature rise values (mean ± SD) during photopolymerization under demineralized and undemineralized dentin disks (n = 10).

Groups Groups definitions Mean ± SD (°C)
Undemineralized dentin Demineralized dentin
1 ΔT Dentin (10 s light curing) 2.39 ± 0.60aA 2.47 ± 0.40aA
2 ΔT Dentin (40 s light curing) 6.26 ± 1.10aB 7.02 ± 0.43aB
3 ΔT LS System adhesive primer (10 s light curing) 2.14 ± 0.31aA 2.34 ± 0.27aA
4 ΔT LS System adhesive bond (10 s light curing) 1.83 ± 0.17aA 1.98 ± 0.24aA
5 ΔT Filtek LS with primer and adhesive (40 s light curing) 5.14 ± 0.62aB 5.45 ± 0.49aB
6 ΔT Filtek LS without primer and adhesive (40 s light curing) 5.58 ± 0.86aB 6.25 ± 1.02aB

Means followed by different letters show statistical differences: (α = 0.05).

Lower case letters: comparison of dentin discs at each procedure (row).

Capital letters: comparison of each photopolymerization step for each kind of dentin (column).

ΔT: temperature change.