Figure 6.

Figure 6

(a) Representative It curve and schematic of the four different deposition regimes. (b) Chronoamperometric curves recorded during growth of Cu nanowires in identical templates (30 µm thick PC, 107 channels/cm2, pore diameter 450 nm) in a solution consisting of 0.25 mol/L CuSO4·5H2O and 2 mol/L H2SO4, by applying different potentials (versus Ag/AgCl/3 mol/L KCl provided with a Haber–Luggin capillary). Adapted with permission from [59] – Copyright 2003 The Electrochemical Society, Inc.