ACB content (○) and SSA of as-prepared composite LiFePO4-ACB (◇), pure ACB (◻), and pure LiFePO4 (⟡) as well as the SSA of LiFePO4-ACB particles after 4 (▽) and 8 hours (△) oxidation in air at 420 °C as a function of the global EQR in the enclosed setup. Core-shell morphology is detected for (1.02 ≤ EQR ≤ 1.07) where the SSA of the composite LiFePO4-ACB material approaches that of pure LiFePO4 particles.