Skip to main content
. 2013 Feb 22;3:1327. doi: 10.1038/srep01327

Figure 2.

Figure 2

(a) Typical APT reconstruction of the high nickel alloy after aging at 500°C for 10 h in vacuum.The atom maps indicate that well-defined spheroidal precipitates are enriched with solute Cu, Ni, Al and Mn. (b) HAADF image of the precipitate distribution in the high nickel alloy after aging at 500°C for 10 h in vacuum.