Skip to main content
. Author manuscript; available in PMC: 2014 Jan 30.
Published in final edited form as: Carbohydr Polym. 2012 Sep 7;92(1):254–259. doi: 10.1016/j.carbpol.2012.08.114

Figure 3.

Figure 3

SEM images of nanofibrous membranes with (a) PCL only, (b) 25% chitosan and (c) 50% chitosan after subjected to water flux for 5 minutes at 1.5 kPa. The scale bars represent 5 μm.