Skip to main content
. 2012 Jul 30;550(4):214–221. doi: 10.1016/j.msea.2012.04.060

Fig. 8.

Fig. 8

Gauss versus mean curvature distributions of the surface of the Mg2Si phase in a volume of (60 μm × 18 μm × 47 μm – see Fig. 5) (a) where all Mg2Si particles in as-cast condition and after 30 min/540 °C are presented, (b) only the largest Mg2Si particle in as-cast condition and after 30 min/540 °C, (c) all particles but the largest Mg2Si particle in as-cast condition and after 30 min/540 °C.