Cytotoxicity of (A) OMA macromers and (B) photocrosslinked OMA hydrogels on hBMMSCs after 48 h as quantified by an MTS assay and normalized by the absorbance of samples at 490 nm to that of the control without any macromer or insert in the medium. Values represent mean ± standard deviation (N = 3) *p > 0.05 compared with OMA-9.