Figure 2.

Figure 2

(a) T2-weighted images of UW-17 MNTs prepared at 5 concentrations in 1-wt% agar gel and (b) their corresponding intensity-decay profiles fit to equation [1]. (c) Linear fit to T2-relaxivity (1/T2) as a function of MNT concentration; slope of fit is r2 [mM−1 s−1].