Skip to main content
. 2012 Oct 30;7(1):604. doi: 10.1186/1556-276X-7-604

Figure 5.

Figure 5

Average roughness (Sa) as a function of Tg for SiOxfilms. Scanned area is 4 × 4 μm2.