Table 1.

Contact Angle of Untreated and Plasma-Treated PLLA Microfibrous Scaffolds and PLLA Membranes Fabricated by Thermal Molding

 
 
Plasma treated
PLLA material Untreated Ar Ar-NH3/H2
Thermally molded membrane 67.7±2.6 53.6±0.6 48.8±0.8
Electrospun microfibrous scaffold 116.2±3.6 85.0±4.3 ∼0

PLLA, poly(l-lactide).