Skip to main content
. Author manuscript; available in PMC: 2014 Feb 21.
Published in final edited form as: Polym Chem. 2012 Nov 26;4(4):1167–1175. doi: 10.1039/C2PY20843A

Fig. 4.

Fig. 4

Conversion versus time plots for the a) EGDMP/DAS system and the b) HDT/DAS system polymerized via redox initiation at 4 BPO concentrations. a) EGDMP/DAS formulated with 0.05 wt%, 0.075 wt%, 0.1 wt%, and 0.2 wt% of BPO and 1:1 [BPO]:[DMT]. The 0.05 wt% and 0.075 wt% samples contained 10:1 [BPO]:[MEHQ], while the 0.1 wt% and 0.2 wt% samples contained 4:1 [BPO]:[MEHQ]. b) HDT/DAS formulated with 0.1 wt%, 0.2 wt%, 0.3 wt%, and 0.4 wt% BPO, 1:1 [BPO]:[DMT], and 10:1 [BPO]:[MEHQ].