Fig. 2.

Fig. 2

Microstructure of deformed iron after seven passes looking parallel to the TD (a and c) and the ND (b and d) presented with grain boundary maps derived from electron back-scatter diffraction measurements showing high-angle boundaries in black (angle >15°) and low-angle boundaries (angle >5°) in red. Additionally electron back-scatter images at higher magnifications are displayed.