Skip to main content
. 2013 Feb 5;13(2):2011–2022. doi: 10.3390/s130202011

Figure 2.

Figure 2.

(a) ATR FT-IR spectra measured on bare PE and PPAA-PE substrate after ddH2O 30 min. rinsing. (b) ATR FT-IR spectra measured on bare glass and PPAA-glass substrate after ddH2O 30 min. rinsing.