Table 1.
Material | Process | Sensor response (-) to acetone [ppm] | LOD (ppm) | Temperature (°C) | Ref. |
---|---|---|---|---|---|
| |||||
Fe2O3/Pt | Wet-method | 4.2 [10] | 10 | 300 | [42] |
Fe2O3/RuO2 | Wet-method | 1.5 [10] | 10 | 300 | [42] |
SnO2 | Dip-coating | 2 [3] | 2 | RT | [43] |
TiO2 | Drop-coating | 4 [1] | 1 | 500 | [23] |
SnO2-ZnO | Wet-method | 2.3 [200] | 200 | 300 | [44] |
Cr-WO3 | Drop-coating | 1 [0.5] | 0.2 | 400 | [25] |
Ce-SnO2 | Dip-coating | 75 [100] | 100 | 210 | [45] |
Si-WO3 | FSP | 4.1 [0.5] | 0.02 | 400 | [26] |
ZnO | RF-SPU | 0.2 [60] | 15 | 400 | [46] |
Sensor response: Rair/Ranalyte − 1; LOD: Limit of detection