Skip to main content
. Author manuscript; available in PMC: 2014 Mar 11.
Published in final edited form as: Soft Matter. 2013 Mar 11;9:4738–4761. doi: 10.1039/C3SM27710K

Figure 16.

Figure 16

(Left) Time-dependent SFG signal intensities at 2840 and 2945 cm−1 as AATM molecules diffuse into d-PMMA films of different thicknesses: (a) 20, (b) 70, (c) 150, (d) 210, and (e) 269 nm. (Right) Diffusion kinetics fitted by the Fickian model. Reprinted with permission from ref. 135. (2004 American Chemical Society)