Skip to main content
. 2013 May 8;14(2):838–846. doi: 10.1208/s12249-013-9970-0

Table III.

The Bead Content After the Electrospinning Process for an Initially Added 10–50% (w/w) of MIP8 Beads in a 40% (w/v) Eudragit-RS100 Solution

Initial polymer beads (%, w/w) Bead content (%)
10 67.00
20 72.73
30 84.22
40 87.21
50 89.55