Table 3. Relaxivity of γ-Iron(III) Oxide Nanoparticles and Magnevist in Deuterium Oxide.
sample | r1 | r2 | r2/r1 |
---|---|---|---|
GdDTPA | 4.81 | 3.84 | 0.80 |
Fe2O3 3.2 nm | 3.00 | 23.75 | 7.92 |
Fe2O3 4.8 nm | 3.52 | 28.26 | 8.03 |
Fe2O3 7.5 nm | 10.8 | 204.2 | 18.91 |
sample | r1 | r2 | r2/r1 |
---|---|---|---|
GdDTPA | 4.81 | 3.84 | 0.80 |
Fe2O3 3.2 nm | 3.00 | 23.75 | 7.92 |
Fe2O3 4.8 nm | 3.52 | 28.26 | 8.03 |