Skip to main content
. 2013 May 30;8(5):e64772. doi: 10.1371/journal.pone.0064772

Figure 1. PEOT/PBT wettability and water uptake.

Figure 1

(A) Contact angle measurements of non heat-treated and heat-treated 4000PEOT30PBT70 block copolymer films using the captive bubble method. Data represents mean ± SD of 20 measurements (N = 3 per condition). (B) Water uptake of non-treated and heat-treated 4000PEOT30PBT70 block copolymer films. Data represents mean ± SD, (N = 3 per condition), *p<0.05, **p<0.01.