Table II.

Thickness and specific surface area of the converted layer formed by reacting silicate (13-93) bioactive glass scaffolds for the times shown in 0.25 M K2HPO4 solution at 60°C and starting pH = 12.0.

Immersion time (day) Thickness (μm) Specific surface area (m2/g)
1 2 ± 1 19 ± 2
3 5 ± 2 30 ± 3
6 13 ± 2 47 ± 1