Table I.
Growth metrics and biochemical content of 4 weeks neocartilage constructs*
| Groups | Diameter (mm) (P = 0.4645) |
Thickness (mm) (P = 0.2384) |
Wet weight (mg) (P = 0.4566) |
Water content (%) (P = 0.7472) |
Cell number (millions) (P = 0.2669) |
|---|---|---|---|---|---|
| Control | 5.21 ± 0.22 | 1.53 ± 0.11 | 29.87 ± 4.93 | 88.75 ± 13.23 | 3.01 ± 2.86 |
| 1st & 3rd weeks | 5.17 ± 0.33 | 1.35 ± 0.25 | 29.65 ± 8.80 | 90.50 ± 12.11 | 4.03 ± 3.26 |
| 3rd & 4th weeks | 5.11 ± 0.23 | 1.40 ± 0.22 | 26.45 ± 2.06 | 87.46 ± 7.93 | 4.24 ± 5.22 |
| 4th week | 5.09 ± 0.33 | 1.48 ± 0.42 | 28.30 ± 7.42 | 87.81 ± 9.52 | 4.46 ± 4.39 |
| Continuous | 5.20 ± 0.24 | 1.45 ± 0.35 | 28.09 ± 10.95 | 88.19 ± 5.43 | 2.64 ± 2.22 |
The effects of hypoxia as a function of application time during the self-assembly of AC (control, 1st & 3rd weeks, 3rd & 4th weeks, 4th week, and continuous hypoxia groups) were examined on gross morphology (diameter, thickness, and WW) and biochemical properties (water content and cell number) after 4 weeks of culture. Values are mean ± 95% CI. No significant differences were detected among controls and hypoxia-treated groups. See Results section for details. Col = collagen.