Skip to main content
. 2013 Apr 25;14(6):2014–2022. doi: 10.1021/bm400356m

Table 2. Thickness and xrSLD from X-ray Reflectometry Data of RcLPS Monolayers at Different Surface Pressures.

  tails
inner headgroup
outer headgroup
surface pressure (mN m–1) thickness (Å) xrSLD (× 10–6 Å–2) thickness (Å) xrSLD (× 10–6 Å–2) thickness (Å) xrSLD (× 10–6 Å–2)
10 11 ± 1 7.93 ± 0.04 14 ± 1 12.20 ± 0.01    
30 18 ± 1 9.73 ± 0.01 6 ± 1 13.08 ± 0.02 11 ± 1 10.38 ± 0.02
45 20 ± 1 9.62 ± 0.01 5 ± 1 13.91 ± 0.02 11 ± 1 10.84 ± 0.04