Figure 2. Hydrodynamic diameter (DH) and zeta (ζ)-potential of the AuNPs.
[1]Measured in de-ionized water at 25°C. The concentration of the AuNP solution is controlled by 1 mM Au. [2]The maximum values for AuNP 1 and AuNP 2 are obtained with different time intervals from 3 to 72 hr (Supporting Information, Fig. S4).