TABLE I.
Ultimate Shear Strength (MPa) |
Apparent Shear Stiffness (MPa/mm) |
Total Energy Absorption (J/m2) |
|
---|---|---|---|
P-Ti | 0.0 (0.0–0.3) | 0.0 (0.0–1.3) | 0 (0–45) |
P-HA | 2.1 (1.5–3.2)a,b | 7.8 (4.2–17.9)a,b | 535 (213–574)a,b |
E-HA | 2.0 (0.7–3.4)a | 9.0 (2.7–16.6)a | 339 (92–618)a |
E-HA-Col | 0.5 (0.1–2.1) | 2.5 (0.6–8.9) | 73 (7–456) |
Data presented as median and interquartile ranges. n = 7.
P-Ti, plasma spray titanium alloy; P-HA, plasma spray hydroxyapatite coating; E-HA, electrochemical-assisted hydroxyapatite coating; E-HA-Col, electrochemical-assisted hydroxyapatite mineralised collagen coating.
p < 0.05 compared with P-Ti.
p < 0.05 compared with E-HA-Col.