TABLE I.

Mechanical Testing

Ultimate Shear
Strength (MPa)
Apparent
Shear
Stiffness
(MPa/mm)
Total Energy
Absorption
(J/m2)
P-Ti 0.0 (0.0–0.3) 0.0 (0.0–1.3) 0 (0–45)
P-HA 2.1 (1.5–3.2)a,b 7.8 (4.2–17.9)a,b 535 (213–574)a,b
E-HA 2.0 (0.7–3.4)a 9.0 (2.7–16.6)a 339 (92–618)a
E-HA-Col 0.5 (0.1–2.1) 2.5 (0.6–8.9) 73 (7–456)

Data presented as median and interquartile ranges. n = 7.

P-Ti, plasma spray titanium alloy; P-HA, plasma spray hydroxyapatite coating; E-HA, electrochemical-assisted hydroxyapatite coating; E-HA-Col, electrochemical-assisted hydroxyapatite mineralised collagen coating.