Skip to main content
. Author manuscript; available in PMC: 2014 May 14.
Published in final edited form as: Chem Mater. 2013 Apr 8;25(9):1968–1978. doi: 10.1021/cm400711h

Figure 7.

Figure 7

Evidence for oxidation during hydrothermal treatment and water storage. (a) mdMS62 samples before and after hydrothermal treatment. (b) Fe edge EELS spectra from a mdMS62-no hy sample after zero and 14 days of storage in DI water. (c) mdMS62 sample before and after hydrothermal treatment in a deoxygenated environment. (d) Percent original r2 of mdMS samples with no hydrothermal treatment and hydrothermal treatment with or without oxygen over time in DI water.