Skip to main content
. Author manuscript; available in PMC: 2013 Oct 21.
Published in final edited form as: Lab Chip. 2012 Oct 21;12(20):4120–4127. doi: 10.1039/c2lc40315c

Table 1.

Bonding time and strength for grafted MAP-TMS/Acrylamide 2:1 molar ratio using either grafting-to or grafting-from polymerization

Bonding Time

Method UV Dose 4 hours 16 hours
Grafting-To 0.144 kJ/cm2 @365 nm 23 psi > 80 psi
Grafting-From 0.325 kJ/cm2 @253 nm > 80 psi > 80 psi