Skip to main content
. 2013 May 16;22(7):1650–1656. doi: 10.1007/s00586-013-2809-2

Table 3.

Fracture pattern exhibited by the specimens after fatigue loading of the spine. After testing there was a total of seven re-fractures in L3 as well as ten adjacent fractures in L2. A combination of fractures occurred in L2 + L3 two times and in L3 + L4 once. Fractures of L4 were rare with only two fractures occurring

Group L2 L2 + 3 L3 L3 + 4 L4
Native 2 2 1 0 0
PMMA 3 0 1 0 1
Modified PMMA 3 0 2 1 0