Skip to main content
. 2012 Feb 14;134(2):24502–NaN. doi: 10.1115/1.4005693

Table 1.

Material parameters of the CJ determined by fitting hysteresis and ramp-hold tests using both Ogden and exponential strain energy density functions

Exponential Ogden
No. A (Pa) B γi τi (s) μ (Pa) α γi τi (s)
1 2.67 0.39 0.44, 0.30 0.97, 112 8.73 2.93 0.41, 0.30 1.02, 117
2 2.15 0.40 0.42, 0.37 1.04, 68.7 7.83 2.87 0.43, 0.31 1.08, 57.5
3 10.0 0.38 0.49, 0.28 0.84, 48.7 30.8 3.25 0.44, 0.31 0.86, 44.7
4 11.6 0.37 0.36, 0.49 1.26, 22.7 39.2 3.30 0.37, 0.49 0.67, 16.8
5 3.45 0.48 0.55, 0.36 0.98, 62.8 9.50 3.11 0.40, 0.35 1.06, 59.5
6 2.39 0.41 0.44, 0.34 1.03, 61.9 9.05 2.89 0.43, 0.34 1.01, 61.9
Mean 5.38 0.41 0.45, 0.36 1.02, 62.8 17.5 3.06 0.41, 0.35 0.95, 59.5
S.D. 3.88 0.04 0.06, 0.08 0.13, 32.7 12.6 0.17 0.02, 0.08 0.14, 36.5
Median 3.06 0.40 0.44, 0.34 1.01, 61.9 9.28 3.02 0.42, 0.31 1.02, 57.5