Skip to main content
. 2013 Jun 26;46(13):5117–5132. doi: 10.1021/ma401014h

Figure 8.

Figure 8

Dynamic viscoelasticity data for thermally cured polybenzoxazines: (a) PBA-a, (b) PBA-a with 5 wt % TDP, (c) PBA-a with 10 wt % TDP, and (d) PBA-a with 10 wt % (TDA). N.B.: scale relates to plot (a) other data offset progressively downward by 1000 MPa for clarity.