Decay of the maximum adhesion during the first 10 contacts of avidin-coated beads on PLL-g-PEG-biotin. The values are normalized with respect to the first contact adhesion of each measurement (10 beads), whereas the bars indicate the standard deviation. The decaying trend was observed for each bead.