Figure 1. NanoART morphology.

Figure 1

Scanning electron microscopy analysis (magnification, 15,000X) of nanoformulations of RTV (H1023 and M1016) and IDV (H1012 and M1002) on top of a 0.2 μm polycarbonate filtration membrane. IDV NP manufactured by homogenization (H10120) had boulder-like shapes and smooth edges, while those manufactured by wet milling (M1002) were ellipsoid with rough edges. RTV NP manufactured by homogenization (H1023) had short rod shapes with smooth edges; while those manufactured by wet milling (M1016) also had short rod shapes, but had rough edges and sharper corners. Measure bar equal 2 μm in all frames.