Skip to main content
. 2013 May 28;13(6):7021–7032. doi: 10.3390/s130607021

Figure 2.

Figure 2.

Contact mode images after indentation tests for a post-deposition cured sample (a) and a pre-deposition cured sample (b). Image (b) shows streaking: gold prepared with pre-deposition curing is so fragile that when the tip reaches the indented area film it starts to scratch. In contrast, indentations could be clearly imaged for post-deposition cured sample (a).