Table 1. Characteristics of electrospun PLLA fibrous scaffolds with G-Rg3 (n = 3).
Sample | Average diameters (µm) | Mass per unit area (mg/cm2) | Porosity (%) | Shrunken (%) |
PLLA | 1.08±0.46 | 1.35±0.18 | 64.5±5.7 | 5.03±0.41 |
PLLA-2% | 1.34±0.62 | 1.28±0.16 | 68.4±4.4 | 3.25±0.29 |
PLLA-6% | 1.21±0.37 | 1.25±0.14 | 64.1±6.4 | 2.86±0.44 |
PLLA-10% | 1.41±0.42 | 1.22±0.16 | 70.1±4.9 | 2.17±0.35 |