Skip to main content
. 2013 Jul 3;6:93. doi: 10.1186/1754-6834-6-93

Figure 6.

Figure 6

Neutron reflectivity data from cellulose films before and after incubation at 75°C with a) 5 μM Cel5A and b) 5 μM Cel5A-CBM.