Table 1.

Size and surface charge for different carboxyl-coated iron-oxide nanoparticles when suspended in either water or RPMI culture media.

Particle source Core diameter (nm) Zeta potential (mv) Hydrodynamic diameter4 (nm)
Water5 Culture media
In-house ~121 −34.5 ± 2.92,a,c 154.7 ± 57.92,b 457 ± 1132,b
Ocean ~203 −51.953 34.8 ± 18.42,b 993 ± 2722,b
NanoTech 31.23
1

Measured by SEM (Zeiss, Merlin SEM).

2

Determined by dynamic light scattering (aZetaPlus analyzer,bHome built, cIn water).

3

Provided by manufacturer.

4

Measured at 10 ug/ml.

5

De-ionized (MilliQ, resistance > 18 MΩ cm).