Figure 4. self-cleaning ability of the (silicate/TiO2)*20 coated stainless steel mesh.

Figure 4

(a) Change of water contact angle of the oleic-acid-contaminated meshes as a function of UV illumination time. (Inline graphic) (silicate/TiO2)*20 coated mesh; (Inline graphic) PDDA/silicate coated mesh; (Inline graphic) original mesh. (Inline graphic) original mesh without oleic acid contamination. (b) Water contact angle changes on the (silicate/TiO2)*20 coated mesh in the five cycles of the oleic acid contamination and UV illumination based recovery. (Inline graphic) (silicate/TiO2)*20 coated mesh; (Inline graphic) after oleic acid contamination; (Inline graphic) after UV illumination recovery.