Figure 3.

Figure 3

HEWL % helicity (y-axis) vs. areal densities (x-axis) of the adsorbed HEWL layers on (a) glass, (b) HDPE, and (c) PMMA. (N=3; averaged 95% C.I. values of ±4 % for helicity and ±0.032 μg/cm2 for areal density.) (Table S.5. in supporting information provides the raw data in Fig. 3.)