Figure 3.

Figure 3

Effects of template micropattern and deposition time on fiber surface coverage and alignment: (a1), (b1), and (c1) schematics of PLLA fiber deposition on PDMS templates with pattern I, II, III, respectively, and SEM micrographs of (a2)–(c3) back side and (a4)–(c6) front side of PLLA fibrous scaffolds.