Electrochemical properties of PrBa0.5Sr0.5Co2−xFexO5+δ in fuel cells (a) Arrhenius plot of reciprocal ASR for PrBa0.5Sr0.5Co2−xFexO5+δ-GDC (x = 0, 0.5, and 1.0) cathode. The inset shows the ASR of PBSCF05-GDC cathode measured at 600°C in air under open-circuit conditions. (b) I–V curves and the corresponding power densities of test cells with PBSCF05-GDC cathode using humidified H2 (3% H2O) as the fuel and ambient air as the oxidant to the cathode at 500 ~ 650°C. (c) Peak power densities of cells with LnBa0.5Sr0.5Co1.5Fe0.5O5+δ-GDC (Ln = Pr and Nd) cathode. (d) Short term stability measurement for a test cell, Ni-GDC | GDC | PBSCF05-GDC, at a constant cell voltage of 0.6 V at 550°C.