Table 1.
Parameter | Crack growth direction
|
p-value | |||
---|---|---|---|---|---|
Transverse | Longitudinal | ||||
K0 (MPa·m0.5) | 0.68 ± 0.16 | 0.67 ± 0.12 | NS | ||
Kg (MPa·m0.5 mm−1) | 1.59 ± 0.23 | 2.48 ± 1.20 | p ≤ 0.05 | ||
Kc (MPa·m0.5) | 1.67 ± 0.40 | 2.01 ± 0.21 | p ≤ 0.01 | ||
Outer | Inner | ||||
K0 (MPa·m0.5) | 0.60 ± 0.14 | 0.81 ± 0.07 | p ≤ 0.01 | ||
Kg (MPa·m0.5 mm−1) | 1.37 ± 0.48 | 1.91 ± 0.26 | p ≤ 0.05 | ||
Kc (MPa·m0.5) | 1.47 ± 0.35 | 1.96 ± 0.28 | p ≤ 0.01 |