Skip to main content
. 2013 Aug 14;8(1):352. doi: 10.1186/1556-276X-8-352

Figure 7.

Figure 7

Hysteresis loops of Co-Ni binary nanowire [Co(II)/Ni(II) = 80:20]. Measured at room temperature using vibrating sample magnetometer.