Mean roughness parameters measured at three different sites on each Epoxy replica.

replica Ra (µm) Rmax (µm) Rpk (µm) Sm (mm) σs (µm) β (µm) η (µm−2) original surface
1 0.193 0.306 0.306 0.048 2.010 24.554 0.045 abrasive paper
2 0.953 1.070 1.070 0.054 4.718 11.253 0.005 abrasive paper
3 1.683 1.587 1.587 0.075 4.137 9.473 0.004 abrasive paper
4 2.287 2.253 2.253 0.075 5.390 7.651 0.003 abrasive paper
5 0.237 0.393 0.393 0.064 4.472 24.439 0.037 microscope slide
6 2.510 2.087 2.087 0.103 2.956 8.058 0.003 office paper
7 1.767 2.173 2.173 0.090 4.426 12.414 0.004 hard paper
8 1.010 0.520 0.520 0.160 8.712 19.859 0.007 hard paper
9 1.793 0.897 0.897 0.358 9.728 20.953 0.011 microscope base
10 4.363 2.807 2.807 0.339 10.327 15.212 0.008 office table
11 1.230 0.927 0.927 0.169 3.818 19.871 0.008 hard paper
12 2.270 1.383 1.383 0.440 7.619 20.977 0.013 plastic folder