Skip to main content
. Author manuscript; available in PMC: 2014 Aug 20.
Published in final edited form as: ACS Macro Lett. 2013 Aug 20;2(8):683–687. doi: 10.1021/mz400256x

FIGURE 3. Polymer 1 degrades in response to both UV-Vis and NIR light.

FIGURE 3

a) GPC traces of 10% polymer 1 before and after irradiation with 320-480 nm light (0 - 60 sec); b) GPC traces of 10% polymer 1 before and after irradiation with 800 nm light (0 – 120 min).