Skip to main content
. 2013 Aug 13;9:1652–1662. doi: 10.3762/bjoc.9.189

Table 1.

Results for the copolymerization of DEAAm and DMAEMA using different monomer ratios.

DEAAm/DMAEMA conc.
[wt %]
AIBN
[mol %]
temp.
[°C]
time
[h]
conversion
[%]
Mn,GPC
[g mol−1]
PDI

1:1 25 0.5 60 18 >99 37200 3.20
5:1 25 0.5 60 18 >99 71500 2.72
1:1 50 0.5 60 18 >99 57100 4.47
5:1 50 0.5 60 18 >99 121400 3.27
1:1 bulk 0.25 varyinga varyinga >99 187400 4.30

a16 h at 60 °C, 8 h at 70 °C, 16 h at 80 °C, and 3 h at 100 °C.